在沥青路面使用时,经过单面烧毛处理后,能更好地与沥青结合,更有效地延长或防止产生裂缝,延长工程使用年限。
To be used road stability for asphalt concrete,the geotextile to be singed Single side,strengthen combined with concrete,effective elongation or preventative to produce crevice elongation the engineering use of time.
序号 Item No.
P010-140
P010-1500
P010-160
P010-180
P010-200
备注 Remark
1
厚度MM≥ Thickness
1.2
1.35
1.5
1.8
2.0
2
断裂强力(纵)KN/m≥ Breaking strength
6.5
7.5
8.0
9.0
10.0
纵横向 WART/WEFT
3
断裂伸长率% Breaking elongation
40-80
纵横向 WARP/WEFT
0.18
0.21
0.23
0.26
0.28
5
CBR顶破强力KN≥ CBR puncture
1.20
1.40
1.50
1.65
1.80
6
等效孔径O90 (O95)mm Across permeability
0.07-0.2
7
235